What PAC does in a drilling fluid
Polyanionic cellulose (PAC) is a water-soluble, anionic cellulose polymer. In water-based muds it does two jobs: it reduces fluid loss by helping build a thin, low-permeability filter cake, and it adds viscosity. Compared with carboxymethyl cellulose (CMC), PAC has a higher degree of substitution, which gives it better tolerance to salt. That is why PAC is widely used in fresh water, seawater and salt-saturated systems.
The grades differ mainly in polymer chain length, and so in how much viscosity they add to the mud.
PAC LV: fluid loss control without extra viscosity
PAC LV (low viscosity) is the choice when you need to cut fluid loss but the mud already has enough viscosity, or the rheology must stay low. Typical cases:
- Weighted muds, where high solids content already raises viscosity
- Systems where yield point and gels are on target, but API or HTHP fluid loss is too high
- Tightening fluid loss late in a section without thickening the mud
- Narrow pressure windows, where extra viscosity would raise equivalent circulating density
PAC HV: fluid loss control plus viscosity
PAC HV (high viscosity) controls fluid loss and builds viscosity at the same time. Typical cases:
- Low-solids and clay-free polymer muds that need carrying capacity
- Salt-water and seawater muds, where bentonite yields poorly and PAC HV supplies viscosity
- Combined with xanthan gum when you need both fluid loss control and low-shear-rate viscosity for hole cleaning
Where PAC RG fits
PAC RG (regular grade) is a general-purpose grade for routine fluid loss control. Ask for the technical data sheet to compare its viscosity and fluid loss performance with LV and HV in your system.
Quick selection guide
| Situation in the mud | Suggested grade |
|---|---|
| Viscosity on target, fluid loss too high | PAC LV |
| Weighted mud with high rheology | PAC LV |
| Need lower fluid loss and more viscosity | PAC HV |
| Low-solids or salt-water mud needing carrying capacity | PAC HV, often with xanthan gum |
| General-purpose fluid loss control | PAC RG (check the TDS) |
Using LV and HV together
Many mud programmes use both grades: PAC HV to set the viscosity profile, then PAC LV to bring fluid loss down to specification without overshooting the rheology. Add PAC slowly through the hopper with good agitation. Adding it too fast forms lumps (“fish eyes”) that waste product.
Temperature and contamination limits
PAC is generally considered effective up to about 300°F (149°C). Above that, thermal degradation increases and high-temperature synthetic fluid loss additives are usually considered. PAC tolerates salt well, but high calcium and magnesium hardness reduce its efficiency, so treat out hardness first where possible, for example with soda ash.
Pilot test before you treat
The right grade and concentration depend on your mud. Run a pilot test on a mud sample: measure rheology and API fluid loss (plus HTHP fluid loss for hotter wells) at two or three concentrations, then choose the treatment. Treatments are often in the range of 0.5 to 2 lb/bbl, but your pilot test result is what counts.
Our R&D laboratory can run these pilot tests for you, and we supply PAC LV, HV and RG with a TDS, SDS and batch certificate of analysis.