First, classify the loss

The loss rate is the first guide to the treatment. A common field classification is:

Loss typeTypical rateUsual cause
SeepageUnder 10 bbl/hrPermeable sands and high-permeability formations
Partial10 to 100 bbl/hrVery permeable zones, small natural or induced fractures
SevereOver 100 bbl/hrLarger natural or induced fractures
TotalNo returnsLarge fractures, vugs or caverns

Thresholds vary between operators, so follow your own loss-circulation guidelines.

Match particle size to the opening

Lost circulation material works by bridging the opening the mud is escaping through, then sealing it. A blend that is too fine passes straight through; one that is too coarse bridges at the face without sealing. For porous formations, a widely used rule of thumb (Abrams’ rule) is that the median particle size should be at least one third of the median pore-throat size. For fractures, the blend needs particles close to the fracture width, plus finer material to fill the gaps between them.

Particle shape matters too. Granular particles form the bridge, flakes lie across openings, and fibres knit the bridge into a mat and reduce its permeability. The most effective treatments usually combine all three.

Seepage losses: treat the active system

  • Add fine to medium fibrous and granular LCM to the circulating system as a background treatment
  • Check shaker screen sizes so the LCM is not removed at surface
  • Good fluid loss control (for example with PAC) and a thin, tough filter cake help reduce seepage into permeable zones

Partial losses: a targeted pill

  • Mix a pill of medium and coarse fibrous, granular and flaked LCM and spot it across the loss zone
  • Reduce pump rate and equivalent circulating density while the pill works
  • If losses continue, increase particle size and concentration in the next pill

Severe and total losses

  • Pump high-concentration pills of coarse blends, often pulled above the zone and squeezed in stages
  • If conventional LCM does not cure the loss, move to specialised plugs such as cross-linked polymer or cement plugs, following the operator’s procedures

Prevention: wellbore strengthening

Correctly sized LCM added before drilling into a known weak zone can help prop and seal small fractures as they form. This approach, known as wellbore strengthening, can reduce losses before they start.

Prove the blend in the lab

Two laboratory tests help choose the right blend before it goes downhole. The permeability plugging test (PPT) uses ceramic discs of known permeability to simulate porous formations. Slotted disc tests use metal discs with slots of set widths to simulate fractures. Both show whether a blend bridges and seals, and at what concentration.

Our R&D laboratory runs PPT and slotted disc tests, and we supply STFLUX™ fibrous, granular and flaked LCM for seepage to severe loss zones.

Have a drilling fluid challenge?

Share your requirement, quantity or well conditions. Our technical team replies within one working day.

Start a Technical Discussion →