Why rheology matters

Rheology describes how the mud flows. It decides how well the mud cleans the hole, how much pump pressure you need, and how much extra pressure the circulating mud puts on the formation. Three numbers from a rotational viscometer sum it up for daily mud checks: plastic viscosity (PV), yield point (YP) and gel strength.

Taking the readings

A rotational viscometer measures the dial reading of the mud at set speeds, usually 600, 300, 200, 100, 6 and 3 rpm. Under API RP 13B-1, water-based muds are commonly tested at 120°F (49°C), and the test temperature is always reported, because rheology changes with temperature.

Plastic viscosity (PV)

PV (cP) = 600 rpm reading − 300 rpm reading

PV mainly reflects the solids in the mud and the viscosity of the base fluid. A rising PV usually means drilled solids are building up. High PV slows drilling and raises pump pressure, so the usual fix is better solids control or dilution, not more chemicals.

Yield point (YP)

YP (lb/100 ft²) = 300 rpm reading − PV

YP reflects the attractive forces between particles while the mud is flowing, and is a main indicator of the mud’s ability to carry cuttings. Viscosifiers such as bentonite and xanthan gum raise YP; contamination can also raise it unexpectedly. Thinners and dispersants lower it.

Gel strength

Gel strength is the dial reading at 3 rpm after the mud has been left static, usually for 10 seconds and 10 minutes (sometimes also 30 minutes). It shows how well the mud suspends cuttings and weighting material when circulation stops.

  • Flat or fragile gels: the 10-second and 10-minute readings are close. Good suspension that breaks easily when pumps start.
  • Progressive gels: the 10-minute reading is much higher than the 10-second reading. Often a sign of high solids or contamination, and can cause pressure surges when breaking circulation.

The low-shear readings

The 6 and 3 rpm readings show how the mud behaves at the low shear rates found in a wide annulus. They are closely watched in deviated and horizontal wells, where cuttings tend to settle on the low side of the hole.

Reading the trend

What you seeLikely causeTypical action
PV risingDrilled solids building upImprove solids control, dilute
YP and gels risingContamination or high solidsIdentify the contaminant, treat or thin
YP and low-shear readings too lowNot enough viscosifierAdd xanthan gum, PAC HV or bentonite
Progressive gelsSolids or contaminationSolids control, chemical treatment

Our laboratory measures full rheology profiles to API RP 13B-1, and we supply the viscosifiers and fluid loss additives used to adjust them, as well as 6-speed viscometers for measuring them.

Have a drilling fluid challenge?

Share your requirement, quantity or well conditions. Our technical team replies within one working day.

Start a Technical Discussion →